Defects of the Porous Brick

Submitted by: Submitted by

Views: 10

Words: 322

Pages: 2

Category: Business and Industry

Date Submitted: 10/12/2015 12:07 AM

Report This Essay

In the production of porous brick, there are many defects in the extrusion process, which have many defects. The reason of each defect is different, and the reasons of the defects are analyzed.Henan Daswell Machinery Co., Ltd,is a professional manufacturer and trader specializing in the research, development and production of construction machinery for nearly 30 years. Our main products are as follows:concrete mixer js series,concrete batching plants,concrete mixer,blocking making machine,concrete pump,etc. 1 mud bar bending One is the mud outlet when it is bent to one side, the outer side of the thick brick, while thin. The main reason is the machine core, mud cylinder mouth, and the spiral reamer is not in the same center Planetary Concrete Mixer Machine, should be corrected. Two is the mud in the shape of a forward, concave place sometimes pulled bad. Main reason is brick crowded at the top of the machine spiral reamer of the main lobe and side lobe not neat, or accessory lobe of serious wear and tear SICOMA Twin-Shaft Concrete Mixers, deal with spiral reamer of the main lobe and side lobe for repair or replacement. 2 mud bar deformation Mainly because the strength of the mud is not enough, the formation of water is too high, to deal with the formation of water to adjust. 3 mud bar The four corners of the clay bar appear to breach, and the tip of the breach is backward. The main reason is in the middle of the mud extrusion speed, one is to lengthen a core in the middle of the core head SICOMA concrete twin shaft mixer, or in the middle core behind the head core rod set a mud blocking pipe to reduce the central mud; the second is to increase machine export into the discharge end of the four corners of the arc, to expand around into mud volume.